Why do pouches that look perfectly sealed after filling still leak in transit? This problem was faced by Malibu, a California-based brand of live resin and diamond sauce disposable vaporizers. Seals were found open in transit, and oil stains were noticed near the top edge of the pouches, even though the pouches had been approved as perfect. The reason for the leakage was not known to the owner, and the reputation of the brand was put at risk with retailers. After experienced experts were searched for, Printing Shell was approached by the founder following positive reviews, and Kevin Ziller, a Senior Packaging Specialist, was consulted, so the returned pouches were examined step by step and the real cause of the leakage was identified. Keep scrolling to learn what the real cause was, how to seal doypack pouches after filling, and which new exception cases were discovered.

Previous Vendor Experience: Packaging Problems the Owner Faced Before Printing Shell 

The founder believed the flat pouches from the previous vendor were perfectly made. The orange and red color bands, the beach artwork, and the round hang hole were all approved, and the custom printed pouches were considered ready for the shelf. Then the shipments were opened, and three complaints were recorded, with a first suspicion listed by Kevin for each.

  • Open top seals: contamination in the seal zone was suspected.
  • Oil stains at the edge: residue from filling was suspected.
  • Unclear responsibility: it was not known whether the pouch supplier or the filling line was at fault.

The freshness of the product was reduced by exposure to air, and the reputation of the brand was put at risk with retailers. An airtight seal and leak prevention were expected by the founder, but these expectations were not fully met, so how to seal doypack pouches after filling was searched for late one night. Moving forward, the confusion was not answered until the investigation was read.

Observation by Kevin Ziller: What Was Good and What Was Not

A doypack without a zipper, closed with a direct top seal, was observed by Kevin, and the line operators were asked about the filling steps, so human error was ruled out. Seal width was measured with a micrometer (screw gauge), jaw temperature was checked with an infrared thermometer, and strength was tested with a tensile tester. The pouch making, the side seals, and the fill amount were found to be perfect, and the weakness was seen only at the top seal. A film of live resin oil and terpenes was found in the seal area, and fusion of the sealing layer was prevented by that film. Higher sealing temperature and pressure were tried, but the weakness was not removed. Cold seals were also produced by drift in jaw temperature and short dwell time, and channel leaks were found where the film was wrinkled at the hard corners of the device. The same contamination is known in powder packaging and liquid packaging, where dust and droplets are left in the seal zone.

Main Problem Figured Out: Correct Filling but Weak End Seals

The fill amount was correct, but the final seal made at the end was found very weak, so the top edge was left only partly fused. Oil residue, cold seals, and wrinkles at the corners of the device were found to be the causes, and leakage and oil stains were seen at the top edge during transit.

Seal Strength and Leak Test Findings

Seal strength was tested under ASTM F88, and the contaminated seals were found far below clean seals. Leaks were revealed under ASTM D3078 at the wrinkled corners, and a seal width of only 3 mm was measured at the top. In plastic doypacks, the inner sealing layer is commonly made of PE, and this layer is directly exposed to oils and terpenes, so fusion is prevented when residue is left on it. The real answer to how to seal doypack pouches after filling was therefore found in the seal zone, not in the heat setting. Explore Custom Plastic Doypack Packaging Bag options for personalized plastic pouches, then move forward to the solutions.

Recommendations from Kevin Ziller: Fixing the Seal at the Source

The recommendations from the packaging expert were to fix the seal at the source are given below:

Step-by-Step Method: How to Seal Doypack Pouches After Filling

Practical steps for how to seal doypack pouches after filling were listed by Kevin, and a reason was attached to each one.

  • Wipe step: the device was wiped before it was placed in the pouch, because contamination is not removed by temperature.
  • Double top seal: a wider double top seal was specified because channel leaks are formed wherever pressure is uneven.
  • Inner layer: a heat-sealable laminate with a contamination-tolerant inner layer of polyethylene (PE) was selected, because bonding is needed even when residue remains. The exact grade is to be verified.
  • Hang hole: the hole was placed outside the seal zone, so the seal is not weakened.
  • Sealers: an impulse heat sealer was used for samples, and a continuous band sealer was advised for the filling line, with cooling time held under pressure, so seals are set before handling.

Recommendation: A Resealable Zipper Instead of Depending Only on the End Seal

It was recommended by Kevin that the closure should not be left to the end seal alone, and that a resealable zipper should be used. Different types of resealable zippers were explained to the founder:

  • Press-to-close zipper: a basic closure that is pressed shut by hand, and no child resistance is offered by it.
  • Slider zipper: a small slider is moved along the track, so reclosing is made easier for repeated use.
  • Tamper-evident zipper: a strip is placed above the closure, so a first opening is shown clearly.
  • Child-resistant zipper: a deliberate action is needed to open it, so opening by children is made difficult.

SELECTION: Child-Resistant Resealable Zipper and the Reason Behind It

The child-resistant resealable zipper was selected. The reasons were that a child-resistant closure had been requested by the founder, the vaporizer was to be opened and closed more than once, and the product was a cannabis device for which child-resistant packaging is expected by regulations. Moreover, the pouch is kept closed by the zipper after the first opening, which could not be done by the end seal.

Printing Shell Introduces Advanced Sealing Equipment for Custom Packaging

Printing Shell continues to strengthen its flexible packaging operations with improvements in pouch-sealing equipment and production quality control. Based in Newark, California, the company is focusing on more consistent heat sealing for custom doypack pouches used in food, retail, and specialised product packaging. The latest sealing equipment upgrade is intended to improve seal consistency, reduce leakage risks, and meet changing requirements across the US packaging industry.

Danial James, Managing Director of Printing Shell, stated:

“Our focus is on improving sealing precision and production consistency. Every pouch must meet the required sealing standards to protect the product throughout storage, handling, and transportation.”

As part of this development, Printing Shell is strengthening its sealing process through impulse heat sealers for sample preparation and continuous band sealing equipment for production requirements. Temperature control, sealing pressure, dwell time, and cooling under pressure are reviewed during the process. Seal integrity is also assessed through ASTM F88 seal-strength testing and ASTM D3078 leak testing. These measures were particularly relevant during a project for Malibu, where oil residue, inconsistent sealing conditions, and wrinkles near pouch corners were identified as contributing factors behind leakage complaints.

“My motto is strong packaging, clear addressing.” — Halldór Laxness

Additional Suggestions and the Reasons Behind Them

A single option was not relied on, so more steps were suggested to the founder. A filling funnel was proposed, so oil is kept away from the pouch opening. Seal integrity testing was advised on every lot, because weak seals are caught early in this way. Varnish was removed from the seal zone because bonding is blocked by varnish. The same step is applied to every lot of a bulk order, so the first pouch and the last pouch are sealed in the same way. Planning a large run? Explore Wholesale Doypack Packaging, where pouches are supplied with reliable zippers and the same seal tests are repeated on every lot, so a big order is not left to chance.

Updated Demands: The Founder Approved the Doypack Format

After the reasons were understood, approval was given by the founder. The stand-up format was approved, the beach artwork and the hang hole were kept, and a child-resistant closure was requested. A zipper closure and a tear notch were added, a tamper-evident seal was specified, and custom pouch dimensions were chosen for the 2-gram device.

California requirements were also checked. It is reported that cannabis goods are required to be in child-resistant, tamper-evident, and resealable packaging when more than one serving is contained, and that single-use child-resistant packaging is allowed for vape products with the statement “This package is not child-resistant after opening.” Child-resistant packaging is certified under the federal Poison Prevention Packaging Act (16 CFR 1700). These details are to be verified against official DCC guidance and are not legal advice. Explore Sachet Doypack Personnalisé options for personalized sizes, closures, and printing before the designers are met.

Meeting the Designers: Justin Daniel and William John Prepared the Mock-Up

After the discussion between Kevin and the designers, mock-ups were prepared by Justin Daniel, a packaging designer at Printing Shell, according to the choices of the founder. The dieline was defined by William John, and the seal zone was kept free of varnish so that a strong seal is formed. A layout of retail-ready packaging was kept, and the position of the hang hole was verified on the dieline.

How the Design Was Developed: From a Cannabis Theme to the Beach Artwork

At the start, the artwork was planned around a cannabis theme by the designers, but the beach artwork was finalized in the end, according to the choices of the founder. How this artwork was printed, laminated, and tested is explained in the next section.

Mock-Up Production: How the Artwork Was Printed, Laminated, Sealed and Tested

PET film was printed digitally, and the print was checked before the next step, so the results were seen first. A barrier film and an aluminum foil laminate were bonded in the multilayer structure through dry lamination, and polypropylene (PP) was compared as an alternative inner layer. Pouches were made on a pouch-making machine, devices were filled, and the top was sealed, and the run was done as small-batch production. The same sequence is followed in each trial. Seal strength was tested under ASTM F88, leaks under ASTM D3078, and burst under ASTM F2054. Puncture at the corners was tested under ASTM F1306, and lamination bond under ASTM F904.

Production Challenges and Quality Control Supervision

A challenge was faced during production. A long, slotted hang hole was wanted by the owner for retail display, but a round hang hole was recommended by the team because the pouch had already been made in a very small size. Too little margin around the top seal would have been left by a long slot, and the strength of the seal would have been reduced. The round hang hole was therefore approved, and its position was kept outside the seal zone. Incoming film inspection, jaw temperature logging, seal strength sampling, and supervision of the first lots were put in place, so consistency is kept and contamination of the product is prevented. A similar exception was seen with food packaging, where fat residue is left in the seal zone.

Learn more about Flexible Kraft Pouch Packaging Distributors for structures that are heat-resistant. But which size holds a 2 gram vaporizer? The answer is shared at the end, so scroll to the end to know.

Satisfaction and Approval: The Sample Was Accepted

The mock-up was approved, and satisfaction was expressed by the founder. Shelf life and protection of the product were confirmed as acceptable in the trial. Recyclable packaging was then requested for the next order. Mono-material pouches were discussed, but a loss of barrier was noted, and post-consumer recycled (PCR) material was considered for outer layers. Plastic recycling is made harder by mixed layers, so the trade-off was explained openly. Explore Doypack Recycling before the next order is planned. The importance of how to seal doypack pouches after filling was understood by the founder, because a good seal is the base of every other feature.

Among Cheap Custom Packaging Companies, the offer of Printing Shell is backed by seal reports and free design support, so a low price is never traded for proof. A free quote is arranged as soon as contact is made.

Contact Now

Another Confusion Remains: How Is a Custom Printed Doypack Designed 

The sample was approved, but one more confusion remained, namely how a pouch is designed to be seen and chosen on a retail shelf. This question was taken up in the next blog, where the next journey of a second brand owner was followed. Tena Tea, a US-based brand of Ethiopian spice root tea sold in 50 g pouches, was brought to Printing Shell, and how to design custom printed doypack pouches for retail was the question to be answered. In that journey, the design confusion was the main concern, since the front panel was seen for only a few seconds on a shelf. Further exceptions are covered for coffee packaging and snack packaging, where the artwork is required to be matched with the barrier. Let’s discover how 10 goals were achieved from 1 discussion with Kevin Ziller (Packaging Expert at Printing Shell for for 6 years). Learn More

Conclusion

Positive feedback was received from the founder after the revised packaging was approved. During a follow-up discussion six months later, the packaging results and the performance of the revised seals were reviewed. The conversation highlighted the importance of a clean seal zone, a wider double seal, a suitable inner layer, and consistent quality checks. For brands worldwide, this case demonstrates why pouch structure, material selection, and sealing specifications should be assessed according to product weight, filling conditions, and storage requirements before bulk production. These checks help reduce the risk of leakage, damage, and avoidable packaging issues.

Frequently Asked Questions (FAQs)

1. How to seal doypack pouches after filling?

The seal zone is kept clean of oil, powder, and dust before sealing is started. A wide seal is then made with controlled temperature, pressure, and dwell time, and the seal is cooled under pressure so the bond is set firmly. A sample pouch is also tested before the full batch is sealed.

2. Why do seals open in transit?

Fusion of the inner layers is prevented by residue in the seal zone and by cold seals, so weak seals are formed. Vibration, stacking pressure, and rough handling are then faced during shipping, and the weak seals are opened by them. Clean seal zones and tested sealing settings are therefore ensured before dispatch.

3. Which temperature is used for heat sealing?

A range of 140 °C to 160 °C is commonly used, with about one second of dwell time. The exact setting depends on the thickness of the laminate and the sealing layer, so it is confirmed through seal-strength tests on filled samples before production is started.

4. Which sealer is suited for the filling line?

An impulse heat sealer is used for samples and small test batches, since the setup is simple and the cost is low. A continuous band sealer is advised for the filling line, because a steady speed, consistent temperature, and uniform seals are needed for bulk production.

5. How wide should the top seal be?

A width of 8 to 10 mm is generally recommended for the top seal, since a stronger bond is formed by a wider seal area. A double seal is added where leaks are a risk, for example with fine powders, liquids, or heavy fills.

6. Which tests are asked for before approval?

Seal strength (ASTM F88), leaks (ASTM D3078), burst (ASTM F2054), puncture (ASTM F1306), and lamination bond (ASTM F904) are tested on filled samples. The results are reviewed together, and production is approved only after every value is found to be within the required range.

8. Is a zipper needed on a sealed pouch?

A zipper is added for multi-use packs, so the pouch is reclosed after each opening. The top seal is placed above the zipper, so the product is kept sealed until the first opening and tampering is made easier to notice.

9. Is a recyclable pouch possible with strong seals?

Good seals are obtained with a mono-PE structure, since the same material is used on both sides of the seal. However, the barrier is checked first, because moisture and oxygen protection is reduced by some mono-material films, and the shelf life of the product is affected by this.